Shrink Fitting

Expands the outer component so it can be fitted, then grips as it cools.

Shrink Fitting
Shrink Fitting · Industrial Maintenance, Automotive

Bearings, gears, couplings and rail wheels are assembled with an interference fit. The outer component is heated until its bore expands enough to slide onto the shaft, then left to cool and grip.

Induction heating is fast and even all the way around the component, so expansion is symmetrical. Uneven heating makes the bore go oval and the fit jams partway on.

Temperature is controlled so it never passes the limit that would damage the component's heat treatment — a real risk when a torch is used.